Multi-way valve bodies investment cast in CW602N dezincification-resistant brass, with the threaded ports, front flange and mounting lug cast as one piece and the flange face, bore and thread bosses machined to customer drawing.
Investment-cast multi-way valve body in CW602N brass, with the side and top threaded ports, the front port flange, the through bore and the bottom mounting lug produced as one casting. The flange face, bore, port faces and threads are machined to approved drawings for potable water, heating and general fluid control.
| Material Grades | CW602N Brass (CuZn36Pb2As, DZR); C87850 lead-free silicon brass option |
|---|---|
| Product Category | Valve Components / Copper Alloy Castings |
| Casting Process | Investment Casting (Lost-Wax) |
| Geometry | Multi-port valve body with threaded side and top ports, a front port flange with bolt holes around a bore, and a mounting lug; port centres, thread size and bolt pattern defined by customer drawing |
| Machining Support | Turning, Milling, Drilling, Tapping; flange face and bore, port faces and threads finished to approved drawings |
| Surface Finish | As-cast with machined faces; polished, sandblasted or shot-blasted where specified by drawing |
| Tolerance | ±0.2mm casting allowance; flange squareness, bore roundness and thread gauge checked at final inspection |
| Certification | ISO 9001; material records can be arranged by agreement |
| Order Quantity | Reviewed after drawing and quantity confirmation |
| Lead Time | Confirmed after drawing review and scheduling; sample timing evaluated separately |
| Customization | All castings custom made based on customer drawings |
Send us your drawings or specifications for a free quotation after drawing or requirement review.
Get a Free Quote WhatsApp UsThis is a multi-way valve body for water and general fluid control, investment cast in CW602N brass. The side and top threaded ports, the front port flange, the through bore and the bottom mounting lug are poured as one casting, so there is no brazed or screwed-in port stub and the pressure boundary stays in one piece.
Brass is used here because the body is machined on every port. The alloy cuts freely, holds a clean thread and stays pressure-tight at the wall sections a valve body needs. CW602N is an arsenic-bearing DZR grade, so the body does not dezincify in potable or slightly aggressive water the way ordinary yellow brass does.
The casting is poured oversize on the flange face, the port faces and the bore, then machined: the flange is faced and bored, port faces are faced square to their own axes, threads are cut to the drawing standard and the bolt holes are drilled. Port centres, thread size, flange pattern and wall section are fixed by the customer drawing.
As shown, the body carries three threaded ports on the sides and top, a front port flange with four bolt holes around a machined bore, and a mounting lug with a drilled hole at the bottom. The model in the photograph is one size of this body family, as-cast on the outside and machined on the flange face, bore and port faces.
Wall section, port boss height, flange thickness and machining stock come from the drawing. Three points are reviewed before the pattern is cut:
Both grades are cast brasses for valve bodies; the difference is the lead content and how the body is expected to behave in water. Grade, temper and test requirements follow the drawing designation.
| Grade | Reference | Key Properties | Typical Fit |
|---|---|---|---|
| CW602N | CuZn36Pb2As · EN 12165 DZR | Arsenic-alloyed dezincification-resistant brass; free-cutting, pressure-tight and holds a clean thread | Potable water, heating and general service valve bodies |
| C87850 | ASTM B584 · Si 2.5–4.0% | Lead-free and dezincification-resistant, with strength and machinability close to leaded brass | Drinking-water fittings and lead-free lists where Pb content is restricted |
CW602N is the default where the body sees potable or aggressive water and cost has to be held; C87850 is used where a lead-free alloy is called for on drinking-water duty or a restricted-materials list. Chemistry is checked per heat by spectrometer, and PMI can be arranged on request.
Port centres, thread size and depth, flange bolt pattern, wall section and machining allowance on the flange face and port faces are checked against the drawing, and gating is laid out before the pattern is cut.
Wax patterns are injected with the port bosses, flange and lug in one piece, gates are attached and the ceramic shell is built and dried in controlled steps.
The heat is melted to the drawing grade and poured at a temperature set for the wall section, with zinc loss and chemistry checked per heat so the port bosses and flange ring fill cleanly.
Shell is removed, gates and runners are cut off, and the casting is cleaned and inspected for surface defects before machining.
The flange face is faced and the bore turned concentric with it, port faces are faced square to their own axes, threads are cut to the drawing standard, and the flange bolt holes and lug hole are drilled to the pattern.
The body is deburred, cleaned and blasted or polished to the finish called for by the drawing; threads and machined faces are protected through handling so no chips or burrs reach the customer.
Thread gauge and thread depth, flange squareness, bore size, port centre positions, wall thickness and overall envelope are checked against the drawing, and casting soundness is reviewed before packing.
Bodies are packed so the threads and the flange face are not loaded in transit, and the threads stay capped until assembly.
Inspection follows the agreed order process; the finished casting is checked against approved drawings and specifications:
Send us your 2D/3D drawings, samples, or valve body requirements for a free custom quotation after drawing or requirement review.
Request a Quote View All ProductsMaintain uniform wall thickness throughout the casting to minimize shrinkage porosity and thermal stress during solidification. Avoid abrupt section changes; use gradual transitions with fillet radii of at least 2-3mm. Minimum wall thickness for investment casting is typically 2mm for small parts and 3mm for larger components.
Design with minimum 1° draft angle for external surfaces and 1.5° for internal surfaces to facilitate wax pattern removal from the die and ceramic shell breakdown. Deeper features may require additional draft.
Always use generous fillet radii at internal corners (minimum R2-3mm) to reduce stress concentration and improve castability. Sharp corners are prone to cracking and porosity during solidification.
Allow 2-3mm machining allowance per surface for machining operations. Critical sealing surfaces and precision bores may require additional allowance. Machining tolerance requirements should be reviewed against approved drawings; as-cast allowance is confirmed by drawing and casting complexity.
Investment casting provides Ra 1.6-3.2μm as-cast surface finish. For applications requiring smoother surfaces, specify polishing, electropolishing, or machining in the drawing requirements.
A: We work with stainless steel (304, 316, CF8, CF8M), carbon steel (WCB), alloy steel, duplex steel (2205), heat-resistant alloys, copper alloys, and specialty alloys. Custom compositions available per specification.
A: Lead time is confirmed after drawing review and scheduling; sample and production timing are evaluated separately.
A: Every heat can be reviewed with spectrometer analysis. Material records, certificates and inspection items are arranged according to the drawing, code or order requirement; third-party inspection can be requested where applicable.
A: Order quantity, tooling cost and pricing are reviewed after drawing and quantity confirmation.
A: Yes, post-machining support can include turning, milling, drilling, tapping and grinding; finished component readiness is confirmed per drawing and order requirements.
Send us your requirements — we review the inquiry and prepare a quotation after drawing or requirement review.