Cast turbine guide wheels and nozzle rings in Inconel 713 and K424 nickel-based superalloys, with integral guide vanes and a machined bore and locating faces.
Investment cast turbine guide wheels in Inconel 713 and K424 nickel-based superalloys. Integral guide vanes with machined bore and locating faces for turbocharger and small gas turbine nozzle assemblies.
| Material Grades | Inconel 713 (cast Ni-based superalloy), K424 (Ni-Cr-W-Ti-Al cast superalloy), heat-resistant steel on request |
|---|---|
| Product Category | Turbine Components |
| Casting Process | Investment Casting (Lost-Wax) |
| Machining Support | Machining support: Drilling, Tapping, Milling, Turning; operations arranged to approved drawings |
| Surface Finish | As-cast, sandblasted or polished finish as required; other finishing options discussed by drawing |
| Tolerance | ±0.2mm casting allowance; machining tolerance confirmed per drawing |
| Certification | ISO 9001; material records can be arranged by agreement |
| Order Quantity | Reviewed after drawing and quantity confirmation |
| Lead Time | Confirmed after drawing review and scheduling; sample timing evaluated separately |
| Customization | All castings custom made based on customer drawings |
Send us your drawings or specifications for a free quotation after drawing or requirement review.
Get a Free Quote WhatsApp UsA turbine guide wheel is the ring of stationary guide vanes that turns and accelerates hot gas onto the turbine wheel. The hub, the vane ring and the outer shroud are cast as one piece, so the vane passages need no assembly and the bore and locating faces can be machined true to each other. Wheels are produced by Wuxi Huayong Metal Technology Co., Ltd. by investment casting in Inconel 713 or K424 nickel-based superalloy, with bore, faces and mounting features finished to the customer drawing.
All guide wheels are custom manufactured from customer drawings or samples: vane count, vane angle and throat area, hub and shroud diameters, bore size and locating faces come from the drawing rather than a catalogue. Designs are reviewed for castability, vane fill and core stability before tooling, because thin vane sections and thick hubs solidify at very different rates. Quality review may include chemistry records, dimensional checks and selected test methods arranged by drawing, code or order requirement.
Guide wheels sit in the hottest part of the machine, so the grade is chosen for creep and oxidation resistance rather than strength alone. Inconel 713 is a cast nickel-based superalloy hardened by gamma-prime precipitation and widely used for turbine blades and nozzle rings; K424 is a Ni-Cr-W-Ti-Al cast superalloy with a similar service role in equiaxed vane castings. Where gas temperature is lower, heat-resistant steels such as HK40 or 310S can be reviewed instead. All heats are verified with spectrometer analysis, and heat treatment is agreed against the drawing or the material specification.
| Material Family | Common Grades | Key Properties | Typical Applications |
|---|---|---|---|
| Stainless Steel | CF8M, CF8, CF3M, CF3, 316L, 304L | Good corrosion resistance, good mechanical properties | Chemical, food, marine, water treatment |
| Carbon Steel | WCB, WCC, LCC, LC2 | Good strength, weldability, cost-effective | Oil & gas, power, general industrial |
| Alloy Steel | WC6, WC9, C5, C12A, 42CrMo | High temperature strength, wear resistance | Power generation, high-temp service, automotive |
| Duplex Steel | CD4MCu, CD3MN, 2205 | High strength, good pitting resistance | Oil & gas, desalination, chemical |
| Copper Alloy | C95400, C93200, C83600, Tin Bronze | Good wear resistance, corrosion resistance | Bearings, gears, marine, decorative |
| Heat Resistant | HK30, HU31, 310S, 309S | High temperature oxidation resistance | Furnace parts, heat treatment, power |
We produce high-precision wax patterns using injection molding. The wax patterns are exact replicas of the final guide wheel, including every vane passage, the hub and the outer shroud.
The pattern tree is repeatedly dipped into ceramic slurry and coated with refractory sand. This process is repeated 6-8 times to build a strong, heat-resistant ceramic shell.
The ceramic shell is placed in an autoclave where steam melts the wax, which drains out. The empty shell is then preheated to 1000-1100°C to remove residual moisture.
Metal is melted in induction furnaces under carefully controlled conditions. The molten metal is poured into the preheated ceramic shells.
After solidification and cooling, the ceramic shell is removed by mechanical vibration and blasting. The individual components are then cut from the sprue.
All castings undergo proper heat treatment to achieve optimal mechanical properties and material structure.
Machining support can be arranged according to approved drawings. Critical dimensions are checked against approved drawings.
Finished components may include surface finishing and arranged inspection such as dimensional review and chemistry records.
Quality review follows the agreed order process; final condition is checked against approved drawings and specifications:
Turbine guide wheels are used wherever hot gas has to be turned and accelerated before it reaches a rotating wheel:
Send us your 2D/3D drawings, samples, or part requirements for a free custom quotation after drawing or requirement review.
Request a Quote View All ProductsGuide vanes are the thinnest section of the casting and the first place to run short of metal. Keep the vane thickness as uniform as the aerodynamic profile allows, taper the trailing edge to a measurable minimum rather than a knife edge, and expect the as-cast vane surface to stay unmachined.
The hub is the heaviest section and the vane ring the lightest, so the joint between them controls shrinkage porosity. Use generous fillets at the vane roots and avoid a thick boss sitting directly against a thin shroud wall.
The bore, the mounting face and the shroud lip normally share one datum. State the run-out or concentricity limit so it can be checked after machining; a guide wheel that is out of true will rub the turbine wheel or load the bearing.
Allow 2-3 mm on the bore, mounting faces and any location spigot, but leave the vane passages as-cast. Adding allowance to vane surfaces only thickens the throat and changes the flow area.
Nickel-based superalloys are stiff at pouring temperature and crack easily in thin sections. Specify the heat treatment and any grain-structure requirement in the drawing, and agree the inspection level (penetrant, radiographic) before tooling.
A: Both are cast nickel-based superalloys used for hot-section guide vanes and blades. Inconel 713 relies on gamma-prime precipitation for high-temperature strength; K424 is a Ni-Cr-W-Ti-Al cast superalloy used in equiaxed vane and blade castings. The choice normally follows the drawing, the gas temperature and the qualified material list of the end user.
A: Yes. Vane count, vane angle, throat area, hub and shroud diameters and bore size are all made to the customer drawing or 3D model.
A: Yes. The hub, vane ring and outer shroud are investment cast as a single part, then the bore and locating faces are machined. Assembled or welded vane rings can be discussed where the design requires them.
A: Chemistry, dimensional and selected penetrant or radiographic inspection can be arranged according to the drawing, code or order requirement; records are prepared under the ISO 9001 quality system.
A: Order quantity is project-dependent: the guide wheel pattern is tooled once, then production quantities are agreed after drawing review.
Send us your requirements — we review the inquiry and prepare a quotation after drawing or requirement review.